Xytron™ U1535E
Unreinforced, Extrusion
Back to results
General Information
Xytron™ is a high performance plastic compound of Envalior, which is based on PPS (polyphenylene sulphide).
Xytron™ offers extremely good chemical resistance, dimensional stability, intrinsic flame retardancy and high stiffness.
Because of its outstanding properties, Xytron™ contributes to an excellent performance in many different applications.
Special features
General Document
Property Data (PDS)
Chemical Resistance Data
Injection Molding Recommendation (one page)
Injection Molding Recommendation (full)
Guideline U1535E & U1530E
Recommendations for machining Xytron
Shelf Life Statement
Delivery Specification
Design Guide
Regulatory Affairs
Absence Declaration Biocidal Products
2023-11-16
Absence Declaration EPA 20 High Priority Substances 2019
2023-11-16
Absence Declaration Food Allergens
2023-11-16
Absence Declaration Nano Materials
2023-11-16
Absence Declaration Ozone Depleting Chemicals
2024-04-25
Absence Declaration PBT chemicals under TSCA section 6(h)
2023-11-16
Absence Declaration PFAS
2024-03-05
Absence Declaration POPs (Persistent Organic Pollutants)
2023-10-27
Absence Declaration Phthalates (2005/84/EC: DEHP, DBP, BBP,DINP,DIDP, DNOP)
2023-11-16
Conflict minerals declaration (EICC, GeSI)
2024-05-15
Packaging, Packaging Waste and CONEG declaration (94/62/EC)
2021-12-06
REACH Registration Statement
2024-03-27
REACH STATEMENT KOREA
2023-11-16
REACH STATEMENT TURKYE
2023-11-16
RoHS Statement (2011/65/EC: Heavy metals)
2024-02-01
SVHC, REACH Annex XIV and –XVII Statement
2024-03-27
Processing technology
Extrusion
Design challenge
Degradation & Stability | Chemical stability
Have a question? Contact us
Rheological properties
Melt volume-flow rate
4
cm³/10min
ISO 1133
Temperature
315
°C
ISO 1133
Load
10
kg
ISO 1133
Melt flow index MFI
4
g/10min
ISO 1133
MFI test temperature
315
°C
ISO 1133
MFI test load
10
kg
ISO 1133
Mechanical properties
Tensile modulus
1550
MPa
ISO 527-1/-2
Stress at break
40
MPa
ISO 527-1/-2
Strain at break
>50
%
ISO 527-1/-2
Charpy impact strength (+23°C)
N
kJ/m²
ISO 179/1eU
Charpy notched impact strength (+23°C)
68
kJ/m²
ISO 179/1eA
Charpy notched impact strength (-30°C)
9.2
kJ/m²
ISO 179/1eA
Thermal properties
Melting temperature (10°C/min)
280
°C
ISO 11357-1/-3
Glass transition temperature (10°C/min)
90
°C
ISO 11357-1/-2
Burning Behav. at 1.5 mm nom. thickn.
HB
class
IEC 60695-11-10
Burning Behav. at 3.0 mm nom. thickn.
HB
class
IEC 60695-11-10
Electrical properties
Volume resistivity
>1E13
Ohm*m
IEC 62631-3-1
Surface resistivity
>1E15
Ohm
IEC 62631-3-2
Other properties
Density
1200
kg/m³
ISO 1183