Durethan® ECOBKV45FN04

45% 玻纤增强, 注塑成型, 阻燃(无卤), 热稳定, 流动性改良, 回收料含量

通用信息

Durethan® is the trade name for our range of engineering thermoplastics based on polyamide 6 and polyamide 66. These polyamides are partially crystalline thermoplastics which offer an ideal combination of properties, especially for technical applications. They provide high mechanical strength and stiffness, good dielectric properties, high resistance to both heat and chemical attack, and good friction and wear properties.
特殊性能
法规
加工工艺
注塑成型

流变性能

成型收缩率(平行)
0.2
%
成型收缩率(垂直)
0.6
%

机械性能

拉伸模量
15800
MPa
断裂应力
160
MPa
断裂伸长率
2.2
%
弯曲模量
15000
MPa
弯曲强度
265
MPa
简支梁无缺口冲击强度(+23°C)
55
kJ/m²
简支梁无缺口冲击强度(-30°C)
50
kJ/m²
简支梁缺口冲击强度(+23°C)
kJ/m²
简支梁缺口冲击强度(-30°C)
kJ/m²
悬臂梁缺口冲击强度(23°C)
10
kJ/m²
最大刺穿力(+23°C)
910
N
刺穿能(+23°C)
3.9
J

热性能

熔融温度(10°C/min)
220
°C
热变形温度(1.80 MPa)
210
°C
热变形温度(0.45 MPa)
220
°C
线热膨胀系数(平行)
0.2
E-4/°C
线热膨胀系数(垂直)
0.7
E-4/°C
燃烧性(1.5mm厚度)
V-0
class
测试厚度
5VA
mm
厚度为h时的5V燃烧性
5VA
class
测试用试样的厚度
1
mm
燃烧性-氧指数
34
%
球压温度
202
°C
灼热丝燃烧指数GWFI
960
°C
GWFI (厚度(1))
0.4
mm
灼热丝燃烧指数GWFI
960
°C
GWFI(厚度(2))
0.75
mm
灼热丝引燃温度GWIT
750
°C
GWIT (厚度(1))
0.4
mm
灼热丝引燃温度GWIT
750
°C
GWIT (厚度(2))
0.75
mm

电性能

相对介电常数(100Hz)
4.3
-
相对介电常数(1MHz)
3.9
-
介质损耗因子(100Hz)
145
E-4
介质损耗因子(1MHz)
150
E-4
体积电阻率
>1E13
Ohm*m
表面电阻率
Ohm
介电强度
40
kV/mm
相对漏电起痕指数
600
V

其它性能

吸水率
3.5
%
吸湿率
1.1
%
密度
1570
kg/m³

材料特性

Drying temperature dry air dryer
80
°C
Drying time dry air dryer
2-6
h
Residual moisture content
0.03-0.07
%
Melt temperature (Tmin - Tmax)
250-280
°C
Mold temperature
70-90
°C

图表