Pocan® S1506

Unreinforced, Injection Molding, Extrusion, Improved Impact

General Information

Pocan® is a high-quality brand of polybutylene terephthalate (PBT) and PBT blends crafted by Envalior. Pocan is known for its impressive resistance to heat and chemicals, outstanding electrical properties, strength and hardness. It is designed to cater to a wide range of industries, including automotive, electrical/electronics, lighting, household appliances, and sports & leisure.
Special features
Regulatory Affairs
Processing technology
Extrusion, Injection Molding

Rheological properties

Melt volume-flow rate
14
cm³/10min
Temperature
260
°C
Load
5
kg
Molding shrinkage (parallel)
2
%
Molding shrinkage (normal)
1.8
%

Mechanical properties

Tensile modulus
1700
MPa
Yield stress
35
MPa
Yield strain
4.5
%
Nominal strain at break
>50
%
Tensile creep modulus (1h)
1400
MPa
Tensile creep modulus (1000h)
700
MPa
Flexural modulus
1600
MPa
Flexural strength
55
MPa
Flexural strain at flexural strength
6
%
Charpy impact strength (+23°C)
N
kJ/m²
Charpy impact strength (-30°C)
N
kJ/m²
Charpy notched impact strength (+23°C)
75
kJ/m²
Charpy notched impact strength (-30°C)
25
kJ/m²
Izod impact strength (+23°C)
N
kJ/m²
Izod impact strength (-30°C)
N
kJ/m²

Thermal properties

Melting temperature (10°C/min)
225
°C
Temp. of deflection under load (1.80 MPa)
55
°C
Temp. of deflection under load (0.45 MPa)
90
°C
Coeff. of linear therm. expansion (parallel)
1.3
E-4/°C
Coeff. of linear therm. expansion (normal)
1.3
E-4/°C
Burning Behav. at 1.5 mm nom. thickn.
HB
class
Thickness tested
1.5
mm
UL recognition
Yes
-
Burning Behav. at 3.0 mm nom. thickn.
HB
class
Thickness tested
3
mm
UL recognition
Yes
-
Oxygen index
22
%
Ball pressure temperature
180
°C
Glow Wire Flammability Index GWFI
650
°C
GWFI (Thickness (1) tested)
2
mm

Electrical properties

Relative permittivity (100Hz)
3.2
-
Relative permittivity (1 MHz)
3.1
-
Dissipation factor (100 Hz)
30
E-4
Dissipation factor (1 MHz)
170
E-4
Volume resistivity
>1E13
Ohm*m
Surface resistivity
>1E15
Ohm
Electric strength
28
kV/mm
Comparative tracking index
600
V

Other properties

Water absorption
0.4
%
Humidity absorption
0.2
%
Density
1200
kg/m³

Material specific properties

Drying temperature circulating air dryer
120
°C
Drying time circulating air dryer
4-8
h
Residual moisture content
0.00-0.02
%
Melt temperature (Tmin - Tmax)
250-270
°C
Mold temperature
80-100
°C